幸福时光 发表于 2004-8-30 23:33:00

讨论一下这个有点难度的膜系!

<P>CWL:422.7 +/- 0.3 nm
    FWHM: 2.0 +/- 0.4 nm
    Transmission: 48% min. peak
    Blocking: OD 4 from 200 to 1150 nm
    Flatness: 3-5 waves per inch or better
    Parallelism: 3-5 arc minutes or better
    Surface Quality: 80/50 scratch/dig
    Dimensions: 25.0 +/- 0.12 mm diameter, 9.4 mm max.thickness,                         21.0mm   min.clear apertureall specs. at room temp and normal A.O.I.</P>
<P>能做如此指标的镀膜厂商,在国内算不算顶级高手啊?</P>
<P>国内还有哪家能成啊?说说方法!
   </P>
[此贴子已经被作者于2004-8-30 16:15:23编辑过]

幸福时光 发表于 2004-8-31 01:18:00

<P><a href="http://bbs.oecr.com/dispuser.asp?id=3533" target="_blank" ><FONT color=#000000>ic5</FONT></A>、<a href=dispuser.asp?name=coatingli target="_blank" >资料</a>
<a href=messanger.asp?action=newtouser=coatingli target="_blank" >留言</a>")'>coating、li</A><a href="http://bbs.oecr.com/dispuser.asp?id=6870" target="_blank" ><FONT color=#000000>sanma</FONT></A>、<a href="http://bbs.oecr.com/dispuser.asp?id=10952" target="_blank" ><FONT color=#000000>李伟华</FONT></A>等你们倒是说说啊!</P>

linmaco 发表于 2004-9-2 07:58:00

<P>兄弟,真有这么行?成本?若便宜,我改天整几个给您做做。不过要您提供材料,全包!</P><P>是否有问题?</P>

zhuhhui 发表于 2004-9-1 22:38:00

我不懂,但我顶~

ttl 发表于 2004-9-2 16:57:00

<P> 用于生物显微上吧?</P><P>要用到金属膜层和介质膜层,设计上是用诱导透射法设计的。</P><P>如果镀膜条件具备的话应该不难的吧。</P>

幸福时光 发表于 2004-9-2 23:47:00

<P>怎么可能便宜啊?</P><P>18000RMB/P,“镀膜条件具备的话应该不难“,呵呵当然不难了</P><P>有好的镀膜机,有好的技术人员,绝对能镀出来!</P><P>谢谢大家的回复!</P>

linmaco 发表于 2004-9-3 05:59:00

不知贵 公司实现这设备是否是日本的,国产光控较差,德国和美国的这种设备光控不到,可否告知?

幸福时光 发表于 2004-9-3 19:06:00

<P>莱宝的机器,我们稍微改装了一下。</P><P>呵呵,谢谢您的回复,很高兴跟您交流。</P>