请教,激光镜反射膜谁能镀?
<P>High damage threshold mirrorsone side AR coated at 1341nm + 1079nm
and the other side coated for reflectivity R at 1341nm and AR at 1079nm.
R= 40%, 50%, 60%, 70%.AR should be0.5% reflectivity. </P>
<P>请能镀的厂家速报价至<a href="mailtinfo@laseroptex.com" target="_blank" >info@laseroptex.com</A>(厂家最好在北京附近,以便沟通)</P>
<P><BR ><BR ></P> <P>可与上海光机所联系一下,他们做强激光薄膜的。021-69918472 找王英剑</P>